The reason for perforation leakage of gathering pipeline in an oilfield was investigated by size measurement, mechanical properties, metallographic structure, X-ray diffraction (XRD), scanning electron microscopy (SEM) and energy dispersive spectrum (EDS). The results showed that the failure form of the spirally submerged arc welded pipe (SAW) was the corrosion perforation caused by local corrosion. The main cause of corrosion perforation was due to the existence of chlorine ion, H 2 O and O 2 in the pipeline transportation medium. A large cathode and small anode electrode corrosion formed in the pipe marking area and the base metal, which eventually led to the perforation of the steel pipe.
Type of Medium:
Online Resource
ISSN:
1662-9752
DOI:
10.4028/www.scientific.net/MSF.993
DOI:
10.4028/www.scientific.net/MSF.993.1209
Language:
Unknown
Publisher:
Trans Tech Publications, Ltd.
Publication Date:
2020
detail.hit.zdb_id:
2047372-2