Abstract:
The title composite is prepared from mixtures of V 2 O 5 , Li 2 CO 3 , NH 4 H 2 PO 4 , and meso‐tetraphenyl porphyrin as the carbon source (350 °C for 4 h followed by sintering at 800 °C for 8 h in N 2 atmosphere).