ISSN:
0887-6266
Schlagwort(e):
poly(ethylene terephthalate), amorphous, planar deformation of
;
deformation of PET by stretching and forging
;
drawing techniques and deformation of PET
;
crystallization in drawn PET
;
Chemistry
;
Polymer and Materials Science
Quelle:
Wiley InterScience Backfile Collection 1832-2000
Thema:
Chemie und Pharmazie
,
Physik
Notizen:
The planar deformation of amorphous poly(ethylene terephthalate) (PET) was performed by stretching and by forging under comparable conditions at a series of constant temperatures, 80, 90, 100, and 110°C. The highest planar draw ratios of 4.5 × 4.5 and 3.5 × 3.5 were obtained by forging and stretching, respectively. Samples were studied before and after deformation by wide angle x-ray scattering (WAXS), differential scanning calorimetry (DSC), density measurements, and elastic recovery at 100°C. A distinct difference in efficiency of draw between these two techniques is found, as judged mainly by the straininduced crystallization. The forging is more effective than stretching in achieving stabilized planar draw under comparable process conditions.
Zusätzliches Material:
5 Ill.
Materialart:
Digitale Medien
URL:
http://dx.doi.org/10.1002/polb.1992.090300705
Permalink