Advanced Functional Materials, Wiley, Vol. 19, No. 24 ( 2009-12-23), p. 3880-3891
Abstract:
Three groups of free‐standing chemical vapor deposition (CVD) diamond films formed with variations in substrate temperature, methane concentration, and film thickness are analyzed using high‐resolution electron back‐scattering diffraction. Primarily {001}, {110}, and {111} fiber textures are observed. In addition, corresponding primary and higher order twinning components are found. As interfaces, high angle, low angle, primary twin, and secondary twin boundaries are observed. A growth and a twinning model are proposed based on the sp 3 hybridization of the bond in the CH 4 molecule that is used as the deposition medium.