In:
CrystEngComm, Royal Society of Chemistry (RSC), Vol. 24, No. 9 ( 2022), p. 1738-1743
Abstract:
The bending strength anisotropy on the (001) plane or between the (100) and (001) planes of KDP crystals was investigated via a three-point bending test. Fracture surfaces were observed. Moreover, the defect distribution of the KDP samples was also analyzed. The results indicated that the bending strength along the [001] direction was higher than that along multiple directions on the (001) plane, showing pronounced anisotropy. However, the bending strengths along different directions on the (001) plane were similar. For the fractured samples with different orientations, multiple fracture surfaces for the (001), (100), (110), (2̄10), (310) planes were observed. It was also deduced from the linear elastic fracture mechanism that the surface or internal defects with a dimension of 0.1 mm existed in the samples.
Type of Medium:
Online Resource
ISSN:
1466-8033
Language:
English
Publisher:
Royal Society of Chemistry (RSC)
Publication Date:
2022
detail.hit.zdb_id:
2025075-7
Permalink